2. Iziphene ze-nickle (NI) Ukuqeqesha:
. Izizathu eziphambili zezi:
a. Emva kokuqiniswa kwesono, ngenxa yexesha elide lokuvezwa komoya we-subserment kunye nomaleko womphezulu kulula ukuba uxinezelwe kancinci, okukhokelela kwiiblubhu emva kokutsala umnxeba; b. Ungcoliseko lwe-Festit c. Xa i-elektroplating, uxinaniso lwangoku lungaphezulu kakhulu; Iindlela zokuphucula ubukhulu becala zibandakanya ngolu hlobo lulandelayo:
a. Emva kokunyanzeliswa, i-porcelain kufuneka igcinwe icocekile kwaye ilungiselele inkqubo yokubeka i-nickel ngokukhawuleza; b. Jonga rhoqo kwaye uhlengahlengise isisombululo sokubeka; c. Xa i-elektroplating, indawo yokuqala incitshisiwe ngokufanelekileyo (umzekelo, yi-2/3 ukuya kwi-3/4 ye-elektrorho eqhelekileyo ye-elektroniki). .
a. Ukuxinana okugqithisileyo kunye nenqanaba lokufundela eliphezulu le-nickel ion; b. Iqondo lokushisa eliphakamileyo kakhulu le-senling lokulinganisa linokukwenza i-mo-nibele c. Ukwakhiwa kotshintsho lwamanzi lotshintsho; The improvement methods are to reduce electroplating current density, to reduce sintering temperature and test & re- treat electroplating solution.
3. Iziphene ze-ceramics egqityiweyo:
1). Amabala amnyama kunye namabala aphuzi avela kumphezulu we-ceramic ecekeceke ngenxa yezi zizathu zilandelayo:
a. I-crystals (ukungcola kweCoramic Comple) njenge-calcium-i-feelspar iguqulwe ibe ngamabala engwevu phantsi kwemeko yonyango lwexesha elide kwiqondo lokutshintsha. b. Kukho iimvakalelo eziguquguqukayo eziguquguqukayo kwi-ceramics ephezulu, enje nge-ti, fe, fe, mn, njl njl. Eyona ndlela iphambili yokuphucula njengoko ngezantsi:
a. Lifinyeze amaqondo obushushu amaqondo obushushu ashushu kangangoko kunokwenzeka, b. Ngokukhethekileyo khetha izixhobo ezingafunekiyo ze-ceramics yezobuchwephesha kwimveliso c. Kunye nokulungelelanisa ubume be-ceramic ngokufanelekileyo. 2). Ezona zinto zingezantsi zezomphezulu we-porcelain engacingiyo ifumana ngwevu kwaye imnyama:
a. I-Direetment Lawer kunye ne-molybdenum wire ye-wire ye-oxidod i-oxidred ibaluleke kakhulu, ebangelwa bucala bubukrelekrele;
b. Ungcoliseko olukhulu lwe-champfer kunye ne-tube yendawo yokuhlala, kunye nokuziqengqeshwa kwempahla, ngakumbi ipropathi yekhabhoni, yenza umphezulu we-ceramic omnyama; d. Iplate ye-Ceramic, i-curundum ye-medicang medings kwaye ukusetyenziswa okuphindaphindiweyo kwezi zinto zincedisayo kukhokelela kwi-volarication ye-adsorption.
Ukuphucula amanyathelo akuyo nje ukulawula ukuveliswa kwe-molybdenum oxide, kodwa kukuphepha i-tube yekhabhoni, i-tubes, i-champoric chamfer, ipleyiti ye-cempora njl njl.
3). Emva kokunyibilikiswa, kukho ezi zizathu zilandelayo zikhokelela ekusetyenzisweni nasekuqhekekeni kweendlela ze-ceramic:
a. Ubunzima obucekeceke, ubuncwane obungalinganiyo, kunye notshintsho oluphambili lobukhulu beengingqi ikakhulu lulula kakhulu ukubangela ukungcungcutheka okanye ukuqhekeka; b. Imveliso kulula ukuyigculela xa ifakwe ngaphandle kwetreyi ye-ceramic sagger; c. Zombini ngaphezulu kwaye ukubamba ixesha elide kakhulu kwiziko kubalulekile ukubangela ukungcungcuthekiswa. d. Utshintsho ekubusweni kwezixhobo zeceramic; e. Ireyitha yokutshutshisa iziko kunye nesantya esipholileyo sizilwe kakhulu, esiya kubangela i-ceramic amalungu aqhekekileyo; Ukwenzela ukuthintela iziphene ezinjalo njengokuqhekeka kwaye ukukhetha, okokuqala kukukhetha iinxalenye ezixineneyo ze-ceramic, ukulila ngokugqibeleleyo ubume bendlela, ukunciphisa uxinzelelo loxinzelelo, kwaye uzame ukuba liyunifoleko. Kule nkqubo, ukufudumeza kunye nenqanaba lokupholisa kufanele kube kufanelekile, kwaye imeko yokunyibilikiswa kufuneka ilungiswe. Xa ubeka izinto ze-ceramic kwiplate ye-ceramic kunye netreyi ye-sagger, kufuneka ilungelelaniswe ngokufanelekileyo kwaye ibe yiflethi kangangoko kunokwenzeka ngokobume kunye nobunzima besakhiwo.
Ishishini le-jinghui ltd lingumenzi we-ceramics, iyeza elibanzi lemveliso kunye neqela elinobuchule, i-veteran kunye nomthengi wethu oqeqeshiweyo, onke amaqhekeza ahlole ngokulandelelana.